TYROLIT is Europe's largest manufacturer of bonded grinding, cutting-off, sawing and drilling tools. Worldwide the TYROLIT Group belongs to the leading system suppliers, which offers grinding tools with bonded abrasives in all conventional grit and bond types as well as a comprehensive range of dressing tools.

The TYROLIT world brands have not only won an outstanding position in their home market. They are worldwide known brand families and represent the performance potential of over 70,000 different TYROLIT products.

Innovation is a driving force in this process. TYROLIT customers profit from extensive advice: economic and ecological solutions are worked out together with TYROLIT.

MIRA is the world's first complete system for grinding and honing operations in gearwheel machining applications.

TYROLIT offers the complete product range:
  • Grinding worms and wheels
  • Internal and external toothed honing rings
  • Standing and rotating dressing tools
  • Grinding tools for internal cylindrical
  • Grinding tools for external cylindrical
  • Cut-off wheels for gearwheel deburring

    GRINDING WORMS for gear flanking machining: Continuous grinding has been accepted as the process of choice for gearwheel fine finishing. We distinguish two continuous grinding methods: generating grinding and contour grinding with grinding worms. Special and sintered aluminum oxides combined with the special VM bond system offer superior profile stability, reduce the stress exposure on the workpiece, increase dressing cycles and shorten grinding times. Minimized diamond dressing tool wear is a distinctive feature of TYROLIT MIRA grinding worms. Non-profiled and precisely pre-profiled grinding worms for continuous generating grinding (e.g. Reishauer RZ 701, RZ 362A systems) are available. Example: Shape 1SCH2G = number of starts: 2 Module range m=0.5 to 8

    HONING TOOLS: Precision gearing and a high removal rate are the convincing benefits of TYROLIT tools for gear flank smooth finishing, e.g. Fässler, Gleason-Hurth, Gleason-Pfauter, Reishauer and Präwema. As the gear flank is machined in hardened state, the percentage contact area and profile tolerances are improved. This translates into a clear noise reduction in operation. Depending on the application requirements, internal geared and external geared honing rings will be used. In connection with the Reifix centering clamping system, the initial dressing infeed is clearly reduced. This increases the overall life of the honing tool.

    SINGLE PROFILE WHEELS for gear flanking machining: With the continuous generating grinding method, it is possible to machine one flank per gap by means of a single flank cut, or both flanks of a gap simultaneously by means of a dual flank cut. The form grinding method requires the grinding wheel to be precision dressed with CNC continuous-path-control.
    Systems: Niles, Höfler, Maag, Gleason Pfauter-Kapp, Samputensili, Reform and Opal.
  •  