Parker Trutec Adds Fourth AFC-Holcroft UBQ Furnace

0
1280

Parker Trutec, Inc. in Springfield, Ohio, recently added a fourth UBQ 36-48-36 universal batch integral quench furnace to an existing line. This furnace will be equipped for carburizing and be made CQI-9 compliant. The equipment was scheduled for installation in March 2016.

Parker Trutec is a North American subsidiary of Nihon Parkerizing, a leading supplier of metal improvement technology. The Parker Trutec Group operates six facilities in the United States and Mexico that specialize in metal treatments and products to improve the resistance to wear, corrosion, and fatigue of metal components. 

AFC-Holcroft is a leading manufacturer of heat treating furnaces comprised of companies that have more than 225 years of thermal processing experience combined. The company manufactures turnkey heat treating systems for applications that include commercial heat treating, bearings, automotive, aerospace, mining, military, aluminum heat treatment, gear manufacturing, fastener manufacturing, and alternative energy industries.

FOR MORE INFORMATION: parkertrutec.com  afc-holcroft.com