February 9, 2012

Share

Gear Solutions
Related Articles

 

Bending Fatigue of Surface Densified Gears - A technical paper discussing the effect of root...

 

Wear Mechanisms of HSS Cutting Tools - The following article provides an overview of the wear...

 

Precision Electrolytic Machining - PEM Technologies presents precision electrolytic machining,...

 

Scuffing Resistance of Isotropic Superfinished Precision Gears - Sikorsky Aircraft, REM Chemicals, Alion Science and...

 

Turbo - Abrasive Machining for Edge and Surface Finishing - In addition to mechanical deburring, turbo-abrasive...

 

No Tools? No Problem. - Its involvement in major hobbing, shaping, and shaving...

 

Case Study: Conicity Technologies - Interested in increasing its cutting tool life, the Getrag...

 

Carbon Coatings for Transmission Components - Sulzer provides a glimpse into the world of diamond-like...

 

Supplier Relationships Speed Gearbox Delivery - Stober Drives’ three-day turnaround on its gearboxes meets...

 

The Case for Cold Rolling - For many gear and spline applications requiring high...

 

Quality Cleaning for Gearing Applications - Just as there are many different methods for cleaning...

 

The Pressure’s On for Decreased Distortion - The goal is to do it well, and do it once, so it’s both...

 

TWIN Blade--A Cut Above the Rest - In the search for optimizing cutting performance, not only...

 

A Green Light to the Future - Ecology Coatings has developed liquid nanotechnology...

 

Surface Enhancement: The Mikronite Process - Not only can this process make your gears stronger and...

 

Harnessing the Horsepower Thief - To achieve a reduction of parasitic friction in automotive...

 

A Hard Turn Toward Efficiency - While grinding is the traditional finishing technique for...

 

The Case for Cold Rolling - For many gear and spline applications requiring high...

 

Determining the Source of Gear Whine Noise - Relating gear pairs to manufacturing errors may lead to...

 

Abrasiveness of Boron Carbide Coatings - Parameters such as coating thickness, counterpart tempering...

 

Surface Coatings for Superior Gears - By Jerry van der Kolk, Christian Strondl, Roel Tietema,...

 

Special Section: Keyseating - In the market for keyseating equipment? With many years of...

 

Abrasiveness of Boron Carbide Coatings - Parameters such as coating thickness, counterpart tempering...

 

Making a Case for PVD Recoating Systems - The following is a case study conducted and prepared by...

 

Optimizing Operating Efficiency - Coatings, surface finishes, lubrication, geometry… all...

 

It's All on the Surface - New materials and technologies are changing the process of...

 

DLC Coatings for Increased Wear Resistance - Bekaert Advanced Coatings outlines how “diamond-like...

 

Archives > June 2006 > Proven Processes for Improving Parts

Proven Processes for Improving Parts

The Iosso-FE and ZN coating processes lend themselves to a wide variety of parts, with gears being chief among them, leading to long life and economic benefits.

By: Don Ortmann


It's rare to come across a manufacturing process or method that first promises multiple increases in productivity, and then delivers even more. One such method is known collectively as the Iosso metal processes, the first of which was developed and patented more than 30 years ago. As can be expected, quite a few refinements and improvements have been made over the years, and the results are repeatable with great accuracy. Processing costs are quite reasonable, as well. The company which provides these process also known as Iosso Metal Processes has an extensive history of coating gears and cutting tools, and the industries served include automotive, medical, aerospace, packaging equipment, food processing equipment, drive system parts, farm and heavy equipment, and plastic injection molding. What are the different process, and how might they benefit your operation? Letís take a look.


Variations on a Theme

The basic Iosso metal process is a chromium alloy treatment that has characteristics far superior to conventional coatings, in terms of extended life and cost efficiency. Specialized versions include the Iosso-FE process, which can be applied to all ferrous based alloys, and the Iosso-ZN process, which is for zinc die castings.
In general, the coating is comprised of many steps, with each carefully and accurately controlled in order to provide the specific results desired. For gears and components or production wear parts, this coating can provide answers to virtually all the common wear-related problems. The Iosso metal processes benefit manufacturers who require parts to have increased hardness, extended wear, lubricity, and corrosion resistance. Additional characteristics of the coated surface are that it is heat resistant, non-magnetic, crack-free, and static-free. There is no peeling, flaking, or spalling. It is anti-soldering, anti-galling, and does not cause hydrogen embrittlement of the base metal, and the coating replicates the original surface finish. Both Iosso-FE and ZN coating coverage is uniform over complex shapes without buildup on sharp edges or corners (Figure 1).

For Ferrous Alloys

he Iosso-FE process can be bonded directly to all iron based metals, tool steel alloys, stellite, stainless steel, brass, bronze, beryllium copper, tungsten carbide, and Ferro-tic carbide. It provides incredible adhesion and a very hard surface. The surface hardness can be brought up six to eight points higher than the hardness of the base or heat treated metal, and the thickness of deposit can be accurately controlled from .000020î to .0005î. The coating is uniform, even over very complex shapes and corners, and there is no buildup, which makes it well suited for gear applications. The coated gears have enhanced wear with an extended life of six to 10 times normal life. This relates not only to a better gear, but less downtime for machinery in which these gears have been incorporated. It will extend base metal life, reduce corrosion, and increase life expectancy. Moreover, its wear qualities are virtually unmatched by any other coating or surface treatment (see micrograph images in Figure 2, Figure 3 and Figure 4).

As an example, tools for producing a long, high-density powder metal lock housing were coated with the Iosso-FE process. The process produced a uniform non-porous and crack-free coating. (Table I) summarizes the number of parts produced with the coated tools, as compared to the number produced by using uncoated, and titanium treated tools. The Iosso-Fe coated tools have significantly outperformed their uncoated and titanium nitride treated counterparts. This is attributed to the reduction in die wall friction, which enabled compacting and ejection pressures to be reduced, thus lessening the wear and tear on the tools. Also, the adherence of the coating on the tools is significantly better than is obtainable with conventional plating, the coating is not embrittled with hydrogen, and it is static free. Other observed benefits include:


• Uniform density distribution
• Elimination of cracks because the strength of the compact was sufficient to counteract low ejection pressures
• Easier withdrawal of core rods and pins during ejection
• Better surface finish on sintered parts
• Better correlation between applied pressures and tonnage indicator on the pressure
• Material and labor cost reduction

Results for other chromium treated powder metal parts are shown in (Figure 2). Uncoated parts failed the wear and corrosion test. However, the parts coated by the Iosso-Fe process readily surpassed this test.


For Hardening Zinc
The Iosso-ZN process is a patented proprietary process to harden zinc wear components and parts. This coating process specifically transforms everyday soft zinc alloy parts into hard, extremely wear-resistant materials. This process is a chromium direct electro-deposition bath, which comprises an aqueous chromic acid and sulfate solution. This coating bonds directly with the zinc alloy surface and provides a new surface which is extremely hard and tough. Designers can now incorporate the die cast technology with the Iosso-ZN process to produce economical components with excellent strength and close, precise tolerances. This process puts conventional zinc die castings into contention to replace many of the expensive previously used alloys. Design engineers can now look to various grades of zinc and have the confidence to implement them into their precision-designed parts, with zinc now becoming an economical and feasible means to manufacture parts.

The Iosso-Zn process is controlled to provide critical mechanical tolerances with superior uniform coverage. With the application of this coating, surface hardness can now be increased to up to 72 R.C. levels. The range of thickness to achieve superior surface hardness is a controlled tolerance from .000050 to .0005 of an inch. The surface finish will replicate the original surface condition.

The graph in (Figure 5) depicts the hardness of six grades of zinc on the Brinell scale. (Figure 6) depicts the R.C. hardness of the same six grades of zinc after being coated with the Iosso-ZN process.


Easy Evaluation

The processes described can be applied to items varying in size from a 3/16” OD gear to a six-foot shaft. Production wear parts can include gears, shafts, pinions, cams, rollers, valves, pistons, roll forming dies, blades, knives, cutters, slitters, scissors, molds, dies, cavities, cores, ejector pins, punches, cutting tools, and a wide variety of lock parts. The coating coverage is completely uniform and the deposit is maintained to close tolerances, even for very small gears and the sharpest of blades. Critical parts that require extra handling and high-volume component parts are not an issue.

Evaluating contending parts is easy. Prospective customers may send samples along with a blueprint pointing out critical areas, with specifications on tolerance and annual quantities. Once we have evaluated the part and determined its feasibility, a prototype production run is conducted. Turnaround time for processing test quantities is usually one to two weeks. The Iosso laboratory keeps several parts for metallurgical tests, and the balance is returned for customer evaluation.

Every company is looking for less expensive ways of manufacturing in order to increase productivity and profits. The Iosso metal processes are one way of achieving this, since the coating offers multiple increases in part life, less downtime, and an economical manufacturing process.

 

 

About The Author
Don Ortmann is operations manager for Iosso Metal Processes, which is based in Elk Grove, Illinois. He can be reached at (847) 437-8400 or iossometal@iosso.com. Visit online at [www.iosso.net].
 

 